Welcome to The Hand Lettering Forum! This is an interactive Bulletin Board on the topics of Sign making, design, fabrication, History, old Books and of coarse Letterheads, Keepers of the craft. The Hand Lettering Forum features links to resources, sign art history, techniques, and artists profiles. Learn more about Letterheads at https://theletterheads.com. Below you'll see Mchat has been added as a live communication portal for trial, and the Main forum Links are listed below.
a new Hope for High Heat Temp Spray On Chrome, this time over plain old steel tubing instead of stainless steel, new high heat baseocat... seems like the clear has been holding well for the last 2 days.... tomorrow I´ll be chroming it in a Blue color....
after the dish soap cleaning, all you do is rinse with normal water(no need of Di right untill the silvering process) then comes the wetting agent http://www.youtube.com/embed/PgxacQOg_mY
after the Wetting agent rinse with normal water and start pumping the sensitizer(did make a video of it sorry) after 20 seconds start rinsing with normal water, but do a one more rinse with Di water, allow the water to drip for about 5 seconds(never let it dry) then start pumping your Silver...
I didnt want that heat pipe to be just like any other chromed heat pipe... so I clear coated the piece with my favorite of colors..Blue, Blue Candy that is...